[Ferro List] dougs fc

xoutpost at netscape.com xoutpost at netscape.com
Sat Apr 12 09:46:42 MDT 2008


 the tight bond between the mortar and the lath due to the low-shrink mix and the tight bond between the lath and the internal welded wire cubical structure that also reinforces the 30 pcf 600 psi closed cell neat cellular concrete fill that occupies a 12 inch thick cavity.

hi doug,

i had actually looked at your web site a few days before i came across fc/aereated site,
but did not see specific details on your process, so i just figured that they were more or less similar.
Maybe i missed a page or something?

I would have liked to go to the better living... seminar, if my schedule allowed had the time for the drive.
It has been a while since i was in new meixco.

On your construction process, do you fill the cavities first with cellular, andf then spray the fc second?


Do you do work in parts, or complete all at once.?

Is the roof 1 oot thick also?

About the "internal welded wire cubical structure", I thought you were making lath,#9 6x6x6 boxes and then
tying them together, are you welding them?


thanks
chris
tecumseh,oklahoma












 


_____________________________________________________________
Netscape.  Just the Net You Need.



More information about the List mailing list